CG-202 (CAS 5089-70-3, EINECS 225-805-6, TEC) Gamma-chloropropyl-triethoxy-silane / CPTEO
- Product Details
Keywords
- CG-202 (CAS 5089-70-3, EINECS 225-805-6, TEC) Gamma-chloropropyl-triethoxy-silane / CPTEO
- 3-chloropropyltriethoxysilane CG-202 98% factory
- 5089-70-3
Quick Details
- ProName: CG-202 (CAS 5089-70-3, EINECS 225-805-...
- CasNo: 5089-70-3
- Molecular Formula: Cl-CH2-CH2-CH2-Si(OC2H5)3
- Appearance: Colorless transparent liquid
- Application: a kind of rubber processing aids
- DeliveryTime: prompt
- PackAge: Packed in plastic barrels, partition 2...
- Port: Qingdao Port
- ProductionCapacity: 1000 Metric Ton/Month
- Purity: 98%
- Storage: It is sealed and stored in cool and we...
- LimitNum: 1 Metric Ton
Superiority
3-chloropropyltriethoxysilane CG-202 98% Technical Index:
Purity: >98%
Free Chloride: 30ppm
Boiling Point(℃): 218-222
Gravity: (ρ 20℃)1.002-1.006
Refractive Index(ND):1.42±0.005
Viscosity(γ 20℃):1.5-1.56
We are 3-chloropropyltriethoxysilane CG-202 manufacturer. We can produce it 1000 ton/month. Now it is in stock.
Details
1.Chemical Name: 3-chloropropyltriethoxysilane CG-202
2.CAS No.: 5089-70-3
3.Molecular Structure: Cl-CH2 -CH2 -CH2 -Si(OC2H5)3
4.Molecular Weight: 240.5
5.Physical & Chemical Properties: It’s colorless transparent liquid,dissolved in ethanol, ketone and benzene, hydrolytic while it’s with water.
6.Technical Index: Purity: >98%
Free Chloride: 30ppm
Boiling Point(℃): 218-222
Gravity: (ρ 20℃)1.002-1.006
Refractive Index(ND):1.42±0.005
Viscosity(γ 20℃):1.5-1.56
7.Usage:
As a kind of rubber processing aids, it is used to couple a wide range of rubber halides such as chloroprene rubber, chlorinated butyl rubber, chlorohydrin rubber, chlorosulfonated polyethylene. It is made into pale products to enhance comprehensive both physical and chemical functions. In addtion, it plays the role as a basic raw material of Si-69 and KH-550.
As a kind of rubber-processing aid, it can be used to treat and couple the inorganic
fillers in halogenated rubber, which includes chlorobutadiene rubber, chlorinated
butyl rubbber,chloro hydrine rubber, chlorosulfonated polyethylene etc.,so as to
improve their physical-mechanical properties.
8.Package
Packed in plastic barrels, partition 250kg or 1000kg, or iso tank container.